Wrap Reel Machine
Wrap Reel Machine is used to prepare lea (120 yards) yarns for ascertaining the count strength.
Wrap Reel Machine Specification
- Product Category: QC
- Machine Category: Yarn
- Product Name:Wrap reel.
- Product Model: According to Manufacturer
- Product Class: New
- Origin: England
- Brand/ Manufacturer: James H. Heal & Co. Ltd
- Agent in Bangladesh: No/Yes
- Power:380v
- Temperature:Normal
- Certification:SGS/Others
- Production Capacity:NA
Winding Process of Yarn
Winding speed should be around 1250 meters/ min.
Machines with tension management are preferred.
Clearers settings should be as close as possible. Loephe Yarn master setting is given below:
- N -4.0 (nep) :
- DS-2.0 (short):
- LS-1.6 (short):
- DL-1.18 (long):
- LL-40: (long)
- -DS-14 %( thin):
- -DL-40(thin)
Since loephe has a facility of class clearing. “C” is to be added in such a way that following faults which are displayed in Loephe class clearing should be cleared.
- A4,A3,B4,B3, B2(50%),C1,C2,C3,C4,D1,D2,D3,D4,E,F,G,H1(50%),H2,I1,I2
- Count channel setting should be less than 7%.
- Setting for cluster faults should be set such that, if yarn is produced without bottom apron, or damaged rubber cots is fed, it is cut by clearer.
- Long thick faults in the cone yarn should be zero.
- Long thin faults should be zero.
- If the waxing attachment is below the clearers, the clearers should be cleaned once in a day.
- Splice strength should be more than 75% of yarn strength.
- Splice appearances should be good & all splicers should be checked at least once in a week.
- Good quality wax should be used.
- Wax pick up should be around 0.1%.
- Uniform application of wax to ensure uniform coefficient of friction (0.125 to 0.15).
- Uniform moisture in the cones is important, because coefficient of friction varies as a function of moisture.
- All wax rollers should rotate properly.
- Repeaters should be as low as possible, as this affects package quality.
- It is advisable to produce cones with 1.8 to 2.4 kgs.
- Yarn tension in winding should not be very high.
- Imperfection increase between ring frame & winding should not be over 30% for cotton combed yarns.
More Lab Equipment
- Yarn Appearance Tester
- Manual Twist tester
- Manual Wrap Reel
- Color Matching Cabinet
- Spectrophotometer
- Digital Pilling tester
- Motorized Crock Meter
- Digital pH Tester
- Oven & Incubator
- Sample Dryer
- Sample Dyeing M/C (Rapid)
- Sample Dyeing M/C (AHIBA NUANCE)
- Sample Dyeing M/C (AHIBA NUANCE)
- Electrolux Wascator
- Precision Dryer
- Digital Balance
- Digital Pipette (II)
- Paramount Pick Glass & Scale
- Electric Heater
- Thermo hygrometer
- Perspirometer
Alec, Zhejiang Shenshilei Group Co. Ltd., Email: alec-business@hotmail.com